17-4 (630) Precipitation Hardening
17-4 PH Stainless Steel
UNS Number S17400
C |
Cb |
Cr |
Cu |
Mn |
Ni |
P |
S |
Si |
0.07 max |
0.15-0.45 |
15.00-17.50 |
3.00-5.00 |
1.00 max |
3.00-5.00 |
0.040 max |
0.030 max |
1.00max |